NC Sanding Sealer
SANDING SEALER It’s important to seal wood before TOP COATING it to ensure an even coating — but when you’re going to finish the wood with a clear coating like WOOD POLISH, T.T CLER, you want something extra from the sealer. It should be easy to sand, and should provide a smooth undercoat that bonds well with the finish. Sanding sealer helps to ensure a quality topcoat, but should be used conservatively one or two coats at most — as too much of this soft undercoat can cause a more brittle one, like lacquer, to crack and peel. USE TO THE S.SEALER You spray or brush sanding sealer — depending on the volatility of the product you use — on freshly sanded wood. It typically dries in 30 minutes to an hour, and you then sand it by hand, using 150- or 220-grit sandpaper. The bulk of the product should be sanded off. When you’re done sanding, you prepare for the next finish coat by wiping off the fine soapy residue with a rag
PRODUCT FEATURES
A low viscosity versatile sealer Very quick drying, making it suitable for production line use User friendly & low level of dusting Ease of sanding to produce a smooth finish Designed to have excellent penetration of wood surfaces Recommended as a quick drying sanding sealer for wood designated for painting Can be over coated with alkyd based varnish & Paints, A.C. catalyzed paints & varnish & acrylics
160-180 Sq ft/L/Coat
**coverage may vary based on the type of wood
used and the application methodology
30 minutes application by padding, Flash
point above at 12c.
Drying time 2 minutes
Recoating Interval: @ 30c and 60% RH
Touch Dry